| A quick and effective method
of cleaning objects prior to plating. The cleaning process
uses as |
| electrolytic bath, similar to
plating operations. The 2 lb. (.9 kg) size makes 8 gallons
(30.4 l) - 5 lb. |
| (2.3 kg) size makes 20 gallons
(114 l). Use with a stainless steel anode. Clean with
the solution heated |
| from 120° to 160° F
(50° to 71° C) at 2 to 6 volts for 15 to 30 seconds. |