| Produces a uniform silver plate.
Use with a stainless steel or pure silver anode. Plate
with solution at |
| room temperature at 1.4 to
1.8 volts for 15 to 90 seconds. The finish will reflect
the surface of the |
| underplate; shiny silver over
shiny metals and matte silver over a dull surface. |